Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.7 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.7 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific) Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied.. |
|||
Melt Flow | 9.7 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.7 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML7666 PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 9.7 g/10 min @Load 6.60 kg, Temperature 337 °C |
9.7 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |