Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 70 - 85 g/10 min @Load 2.16 kg, Temperature 210 °C |
70 - 85 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 3251D Injection Grade PLA IngeoTM Biopolymer 3251D is designed for injection molding applications. This polymer grade has a higher melt flow capability than other IngeoTM resins currently in the market place. The higher flow.. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 330 °C |
70 g/10 min @Load 4.76 lb, Temperature 626 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT1143 PC (Asia Pacific) XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited .. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 330 °C |
70 g/10 min @Load 4.76 lb, Temperature 626 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT1143 PC (Europe-Africa-Middle East) XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited .. |
|||
Melt Flow | 70 g/10 min @Load 2.16 kg, Temperature 230 °C |
70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Kuraray SEPTON® S2002 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Melt Flow | 70 g/10 min @Load 5.00 kg, Temperature 266 °C |
70 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Melt Flow | 70 g/10 min @Load 5.00 kg, Temperature 265 °C |
70 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |