Physical Properties Metric English Comments
Melt Flow 70 - 85 g/10 min

@Load 2.16 kg,
Temperature 210 °C
70 - 85 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
NatureWorks® Ingeo™ 3251D Injection Grade PLA
IngeoTM Biopolymer 3251D is designed for injection molding applications. This polymer grade has a higher melt flow capability than other IngeoTM resins currently in the market place. The higher flow..
Melt Flow 70 g/10 min

@Load 2.16 kg,
Temperature 330 °C
70 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® XHT1143 PC (Asia Pacific)
XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited ..
Melt Flow 70 g/10 min

@Load 2.16 kg,
Temperature 330 °C
70 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® XHT1143 PC (Europe-Africa-Middle East)
XHT1143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is the lowest heat, UV stabilized product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited ..
Melt Flow 70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Kuraray SEPTON® S2002 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
Melt Flow 70 g/10 min

@Load 5.00 kg,
Temperature 266 °C
70 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
Melt Flow 70 g/10 min

@Load 5.00 kg,
Temperature 265 °C
70 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications