Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 60 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 200 °C
60 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE)
Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi..
Melt Flow 60 g/10 min

@Load 10.0 kg,
Temperature 190 °C
60 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PE 1295
PRE-ELEC PE 1295 is a dissipative thermoplastic compound based on PE-HD. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance bet..
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 230 °C
60 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PP 1375
PRE-ELEC PP 1375 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Melt Flow 60 g/10 min

@Load 21.6 kg,
Temperature 200 °C
60 g/10 min

@Load 47.6 lb,
Temperature 392 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties..
Melt Flow 60 g/10 min

@Load 10.0 kg,
Temperature 220 °C
60 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
LG Chemical 81HF SAN Resin
High flow, Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include food receptacles, disposable li..
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 265 °C
60 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East)
VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles.
Melt Flow 60 g/10 min

@Load 6.60 kg,
Temperature 337 °C
60 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr..
Melt Flow 60 g/10 min

@Load 10.0 kg,
Temperature 220 °C
60 g/10 min

@Load 22.0 lb,
Temperature 428 °F
from MVR; ISO 1033
Sax Polymers SAXLAC 420HI Acrylonitrile Butadiene Styrene
Saxalac 420HI is a flame retardant, very high flow ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provided..
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 160 °C
60 g/10 min

@Load 4.76 lb,
Temperature 320 °F
ASTM D1238
Lubrizol Estane® UB410A Thermoplastic Polyurethane
Type: Estane® UB410 is a Shore 70A, polyester based, hot melt adhesive with excellent low temperature flexibility thermoplastic polyurethane (TPU).Uses: Extrusion, Powder Coating.Available in Europ..
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 280 °C
60 g/10 min

@Load 4.76 lb,
Temperature 536 °F
JIS K 6719
Zeon Chemicals Zeonor® 1060R Cyclo Olefin Polymer
Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi..
Melt Flow 60 g/10 min

@Load 21.6 kg,
Temperature 190 °C
60 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Borealis BS4641 High Density Polyethylene
BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App..
Melt Flow 60 g/10 min

@Load 5.00 kg,
Temperature 230 °C
60 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis ME212U Polypropylene Compound, Mineral Filled
ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air..
Melt Flow 60 g/10 min

@Load 10.0 kg,
Temperature 220 °C
60 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO-1133
Chi Mei Polylac® PA-765 ABS - Flame Retardant
F.R. High Flow
Melt Flow 60 g/10 min

@Load 6.60 kg,
Temperature 337 °C
60 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem ATX103R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r..
Melt Flow 60 g/10 min

@Load 6.60 kg,
Temperature 337 °C
60 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..
Copyright © lookpolymers.com All Rights Reserved