Polymer Property : Melt Flow = 5.9 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 5.9 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.9 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS/PC 7901