Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS/PC 7901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |