Polymer Property : Melt Flow = 5.28 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 3.5 - 5.28 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 5.28 g/10 min

@Load 4.76 lb,
Temperature 374 °F
±10%
Kazanorgsintez PE2NT 16-11 Linear Low Density Polyethylene
Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez