Polymer Property : Melt Flow = 3.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Network Polymers Softflex® 5000
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Melt Flow 3.5 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4440R (40404) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 3.5 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4441R (40404) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 3.5 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6432R (32604) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 3.5 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6433R (32604) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 210 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas..
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Kingfa FW-620 Flame Retardant ABS
Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Kingfa HF-618 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Kingfa HP-126 Modified ABS
Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) I4 HD 7255 High Density Polyethylene
HD7255 is a HDPE grade with high impact strength and low warpage.Applications: thick walled, highly stressed transport containers, injection molding.Information provided by Iran Petrochemical Commer..
Melt Flow 3.5 - 5.28 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 5.28 g/10 min

@Load 4.76 lb,
Temperature 374 °F
±10%
Kazanorgsintez PE2NT 16-11 Linear Low Density Polyethylene
Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) EX7C HF4750K High Density Polyethylene
Wire & CableInformation provided by Iran Petrochemical Commercial Co.
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133/ASTM D1238
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Melt Flow 3.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ISO 1133
Styron Pulse® 920 MG PC/ABS
An inherently matt medium heat, medium impact PC/ABS resin, PULSEâ„¢ 920 MG is designed for interior automotive applications where a matt aesthetic is required.Information provided by DowThis pro..
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin
Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin
Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Chi Mei Polylac® PA-716 ABS - High Flow
High flow, medium impact
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 1000
Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc.
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 1002
Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc.
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 2512
Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc.
Melt Flow 3.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3501 GF-10
Description: Reinforced Grade, 10%Glass FilledInformation provided by Diamond Polymers, Inc.
Melt Flow 3.5 - 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 - 6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 3501 SHF
Description: Super High FlowInformation provided by Diamond Polymers, Inc.
Melt Flow 3.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
3.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade
Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high..
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 260 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade
Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a..
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers SAN 263 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 3501 HF
Description: High FlowInformation provided by Diamond Polymers, Inc.
Melt Flow 3.5 - 5.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 - 5.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
UNI EN ISO 1133
Breplast Bretene SPM Thermoplastic Composite, 70% HD + 30% PP
Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A.
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer  (discontinued **)
Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO..
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 1100
Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc.
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 2510
Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc.