Polymer Property : Melt Flow = 48.6 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 48.6 g/10 min

@Load 5.00 kg,
Temperature 300 °C
48.6 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific)
LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa..