Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 48.6 g/10 min @Load 5.00 kg, Temperature 300 °C |
48.6 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific) LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa.. |