Physical Properties Metric English Comments
Melt Flow 30 - 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 - 40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NatureWorks® Ingeo™ 3251D Injection Grade PLA
IngeoTM Biopolymer 3251D is designed for injection molding applications. This polymer grade has a higher melt flow capability than other IngeoTM resins currently in the market place. The higher flow..
Melt Flow 30 - 40 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30 - 40 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio > 50; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 2260M (601F7) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer