Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 30 - 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
30 - 40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 3251D Injection Grade PLA IngeoTM Biopolymer 3251D is designed for injection molding applications. This polymer grade has a higher melt flow capability than other IngeoTM resins currently in the market place. The higher flow.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 260 °C |
30 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 260 °C |
30 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Melt Flow | 30 g/10 min @Load 10.0 kg, Temperature 220 °C |
30 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 330 °C |
30 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 330 °C |
30 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Melt Flow | 30 g/10 min @Temperature 230 °C |
30 g/10 min @Temperature 446 °F |
ASTM D1238 |
Phillips Sumika Marlex® CHP-370 Thermoplastic Polyolefin
(discontinued **) Thermoplastic Polyolefin, Good Stiffness and Impact PerformanceApplications: Automotive Pillar TrimConditioning after Molding: 48 hr at 23°CNominal Shrinkage: 0.8-1.0%Drying conditionsTemperature: .. |
|||
Melt Flow | 30 g/10 min @Temperature 230 °C |
30 g/10 min @Temperature 446 °F |
ISO 1133 |
Phillips Sumika Marlex® CHP-370 Thermoplastic Polyolefin
(discontinued **) Thermoplastic Polyolefin, Good Stiffness and Impact PerformanceApplications: Automotive Pillar TrimConditioning after Molding: 48 hr at 23°CNominal Shrinkage: 0.8-1.0%Drying conditionsTemperature: .. |
|||
Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 260 °C |
30 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY XTPM405 ASA+PC High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color .. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 330 °C |
30 g/10 min @Load 4.76 lb, Temperature 626 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 330 °C |
30 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 266 °C |
30 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
Global XNY-1424 Easy Flow Polycarbonate/Polyester Alloy Information provided by Global Polymers Corporation. |
|||
Melt Flow | 30 - 84 g/10 min @Load 21.6 kg, Temperature 190 °C |
30 - 84 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT 17-5 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 0740 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowHeat StabilizedOzone ResistantProcessability, GoodSoftUV R.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 280 °C |
30 g/10 min @Load 4.76 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
Melt Flow | 30 g/10 min @Load 6.60 kg, Temperature 337 °C |
30 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 30 g/10 min @Load 6.60 kg, Temperature 337 °C |
30 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 30 g/10 min @Load 10.0 kg, Temperature 345 °C |
30 g/10 min @Load 22.0 lb, Temperature 653 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem SF2350 PEI Blend (Europe-Africa-Middle East) High flow Ultem blends for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 265 °C |
30 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Melt Flow | 30 g/10 min @Load 10.0 kg, Temperature 220 °C |
30 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 260 °C |
30 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 30 g/10 min @Load 6.60 kg, Temperature 337 °C |
30 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Melt Flow | 30 g/10 min @Load 21.6 kg, Temperature 190 °C |
30 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityExcellent tear strengthHigh puncture resistanceGood stiffnessExcellent heat sealing proper.. |
|||
Melt Flow | 30 g/10 min @Load 21.6 kg, Temperature 190 °C |
30 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**) Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p.. |
|||
Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 230 °C |
30 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ ED135AI TPO Compound Daplen ED135AI is a 10% mineral filled grade intended for injection molding. ED135AI offers very good balance in stiffness/impact strengthDaplen ED135AI has been developed especially for the car in.. |
|||
Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 265 °C |
30 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 266 °C |
30 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 230 °C |
30 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ KSX65T20 Polypropylene Compound 20% Mineral Filled Daplen KSX65T20 is a 20% mineral filled grade intended for injection molding. Daplen KSX65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSX65T20 offe.. |