Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers Softflex® 6500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 4.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific) Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade. |