Polymer Property : Melt Flow = 4.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 3.5 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4440R (40404) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 3.5 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4441R (40404) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 3.5 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6432R (32604) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 3.5 - 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 - 4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6433R (32604) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer