Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycolac® MG37CR ABS High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 4.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific) High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 280 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 280 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 260 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 260 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 260 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 190 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borclean™ HC312BF Polypropylene Homopolymer for Capacitor Film Borclean HC312BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC312BF does not contain slip, antiblock, antist.. |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 190 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borclean™ HC318BF Polypropylene Homopolymer for Capacitor Film Borclean HC318BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC318BF does not contain slip, antiblock, antist.. |
|||
Melt Flow | 4.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-756 ABS - High Flow High rigid, high flow |
|||
Melt Flow | 4.4 g/10 min @Load 2.16 kg, Temperature 210 °C |
4.4 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |