Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 39 g/10 min @Load 5.00 kg, Temperature 260 °C |
39 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 39 g/10 min @Load 10.0 kg, Temperature 220 °C |
39 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 (G) |
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Melt Flow | 39 g/10 min @Load 10.0 kg, Temperature 220 °C |
39 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 (G) |
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Melt Flow | 39 g/10 min @Load 5.00 kg, Temperature 280 °C |
39 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Melt Flow | 39 g/10 min @Load 2.16 kg, Temperature 300 °C |
39 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific) LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, .. |
|||
Melt Flow | 39 g/10 min @Load 5.00 kg, Temperature 280 °C |
39 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Melt Flow | 39 g/10 min @Load 5.00 kg, Temperature 280 °C |
39 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Melt Flow | 39 g/10 min @Load 21.6 kg, Temperature 190 °C |
39 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Braskem GM5340PR High Density Polyethylene Triple-layer coating for metallic pipes; Umbilical pipes for offshore oil field platforms; Jacketing for wires and for optic fiber metallic cables; Self-propelled irrigation pipes; Localized irrigat.. |