Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 36 g/10 min @Load 1.00 kg, Temperature 235 °C |
36 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 9000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM3729 PC (Europe-Africa-Middle East) LEXAN FXM3729 is an UV stabilized Visual FX Sparkle grade, with an excellent flow. It contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Melt Flow | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
Melt Flow | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Melt Flow | 36 g/10 min @Load 5.00 kg, Temperature 200 °C |
36 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Melt Flow | 36 g/10 min @Load 5.00 kg, Temperature 200 °C |
36 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Melt Flow | 36 g/10 min @Load 1.20 kg, Temperature 266 °C |
36 g/10 min @Load 2.65 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developed for automotive bezel application that requires basecoat + .. |
|||
Melt Flow | 36 g/10 min @Load 1.20 kg, Temperature 266 °C |
36 g/10 min @Load 2.65 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Melt Flow | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
Melt Flow | 36 g/10 min @Load 5.00 kg, Temperature 280 °C |
36 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr.. |