Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 33.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
33.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers Softflex® 2701-1502R Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 33.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
33.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers Softflex® SF 5060 Overmold for Nylon Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 33.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
33.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers Softflex® SF 8900 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |