Melt Flow 33.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
33.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers Softflex® 2701-1502R
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 33.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
33.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers Softflex® SF 5060 Overmold for Nylon
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 33.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
33.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers Softflex® SF 8900
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.