Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 31 g/10 min

@Load 10.0 kg,
Temperature 220 °C
31 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® S705 ABS (Europe-Africa-Middle East)
CYCOLAC S705 is a new generation ABS plating grade, offering semi high heat with a good property balance for impact and flow. CYCOLAC S705 demonstrates excellent electroplatability and a good therma..
Melt Flow 31 g/10 min

@Load 2.16 kg,
Temperature 260 °C
31 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
Melt Flow 31 - 39 g/10 min

@Load 2.16 kg,
Temperature 190 °C
31 - 39 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 2062x (62135) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 31 - 39 g/10 min

@Load 2.16 kg,
Temperature 190 °C
31 - 39 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4028X (28435) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 31 g/10 min

@Load 5.00 kg,
Temperature 210 °C
31 g/10 min

@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
SABIC Innovative Plastics NORYL WCP821 PPE-TPE
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Melt Flow 31 g/10 min

@Load 5.00 kg,
Temperature 210 °C
31 g/10 min

@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Melt Flow 31 g/10 min

@Load 5.00 kg,
Temperature 210 °C
31 g/10 min

@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Melt Flow 31 g/10 min

@Load 10.0 kg,
Temperature 250 °C
31 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade
Information provided by Samsung Cheil Industries.
Melt Flow 31 g/10 min

@Load 2.16 kg,
Temperature 250 °C
31 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
Melt Flow 31 g/10 min

@Load 2.16 kg,
Temperature 250 °C
31 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
Melt Flow 31 g/10 min

@Load 2.16 kg,
Temperature 230 °C
31 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Calculated from Volume Flow Rate of 25 cm<sup>3</sup>/10min.; ISO 1133
DSM Arnitel® EL630 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melt Flow 31 g/10 min

@Load 3.80 kg,
Temperature 280 °C
31 g/10 min

@Load 8.38 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics GELOY XP4025 ASA+PC
Available in a wide range of colors and is recommended for unpainted exterior applications.
Melt Flow 31 g/10 min

@Load 10.0 kg,
Temperature 250 °C
31 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade
Information provided by Samsung Cheil Industries.