Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ 9545-1 Thermoplastic Elastomer (TPE) Versaflex™ 9545-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Melt Flow | 3.6 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.6 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers ABS 4107 Heat Resistant Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA S610 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers |