Physical Properties Metric English Comments
Melt Flow 3.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
PolyOne Versaflex™ 9545-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9545-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Melt Flow 3.6 g/10 min

@Load 10.0 kg,
Temperature 220 °C
3.6 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Diamond Polymers ABS 4107 Heat Resistant Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 3.6 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.6 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA S610
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 3.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 3.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers