Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.8 - 3.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.8 - 3.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4133Q (33403) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 2.8 - 3.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.8 - 3.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |