Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Network Polymers MS 125 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.6 - 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 - 3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 2.6 - 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 - 3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin Eraclene PF 92 is a homopolymer high density polyethylene resin (HDPE) with antioxidants, suitable for pipe application. It is characterized by high rigidity, high impact strength and low swelling... |
|||
Melt Flow | 2.6 - 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 - 3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4318Q (18403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 2.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl HIPS3191 PS This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Appeel® 22D843 Ethylene Acrylate DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable .. |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Melt Flow | 2.6 g/10 min @Load 10.0 kg, Temperature 190 °C |
2.6 g/10 min @Load 22.0 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Pax-Plus™ 3208 Blown Film Resin Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform.. |
|||
Melt Flow | 2.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS TM 35 Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA/PC FA-30 Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® MB/ML 47 HDPE Made for injection molding and special applicationsInformation provided by Unipetrol RPA |