Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.0 - 2.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 2.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Breplast Bretene SP Polypropylene / Polyethylene Composite Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |