Breplast Bretene SP Polypropylene / Polyethylene Composite

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP)
Manufacturer Breplast S.P.A.
Trade Name Bretene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Breplast Bretene SP Polypropylene / Polyethylene Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A.
Physical Properties Metric English Comments
Density >= 0.930 g/cc
>= 0.0336 lb/in³
ISO 1183-1
Melt Flow 1.0 - 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 - 2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
3.0 - 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 - 5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.00 MPa
725 psi
ISO 527
Tensile Strength, Yield 4.00 MPa
580 psi
ISO 527
Elongation at Break 58 %
58 %
ISO 527
Flexural Strength 22.0 MPa
3190 psi
ISO 178
Flexural Modulus 0.868 GPa
126 ksi
ISO 178
Izod Impact, Notched 0.0800 J/cm
0.150 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F
A50; ISO 306