Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
10.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycolac® INP630 ABS INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance.
Provides excellent hi.. |
|||
Melt Flow | 10.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
10.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi.. |