Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.8 - 14.4 g/10 min @Load 21.6 kg, Temperature 190 °C |
10.8 - 14.4 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6752G (526H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 10.8 - 14.4 g/10 min @Load 21.6 kg, Temperature 190 °C |
10.8 - 14.4 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6845G (446H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 10.8 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.8 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXM141R PC FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Melt Flow | 10.8 - 14.4 g/10 min @Load 21.6 kg, Temperature 190 °C |
10.8 - 14.4 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6844G (446H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 10.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® 368 R Crystal Clear Transparent 77851 SAN Description: General-purpose grade with well-balanced properties, suitable for injection molding and extrusion. Especially for applications where highest transparency and low natural color is requir.. |