Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.73 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.73 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Paxon™ 4700 Blown Film Extrusion Resin
(discontinued **) 4700 is a medium molecular weight, high density polyethylene homopolymer film resin. It can be processed on conventional film extrusion equipment.Information provided by ExxonMobil Chemical |