Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.35 - 0.45 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 - 0.45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4131L (314F4) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |