Physical Properties Metric English Comments
Melt Flow 0.35 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.35 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film
Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Melt Flow 0.35 - 0.45 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 - 0.45 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4131L (314F4) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.35 g/10 min

@Load 5.00 kg
0.35 g/10 min

@Load 11.0 lb
ISO 1133
Total Finathene® 1288 HDPE film  (discontinued **)
Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti..
Melt Flow 0.35 - 0.70 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.35 - 0.70 g/10 min

@Load 11.0 lb,
Temperature 374 °F
±10%
Kazanorgsintez PE80B-275 Medium Density Polyethylene Composite
Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc..
Melt Flow 0.35 - 0.70 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.35 - 0.70 g/10 min

@Load 11.0 lb,
Temperature 374 °F
±10%
Kazanorgsintez PE80B-286 Medium Density Polyethylene Composite
Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc..
Melt Flow 0.35 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.35 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene
BL4M is a high density polyethylene with 1-Butene as co monomer. It is high molar mass, easily processable, high stiffness and strength, good SCR, very good molding surface finish.Applications: jer..
Melt Flow 0.35 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.35 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) BL4 HM 8255 High Density Polyethylene
BL4 (HM 8255) is a high density polyethylene with Butene-1 as comonomer. It is a high molar mass, easily processable, high stiffness and impact good stress cracking resistance and even good molding ..
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene G2855 High Density Polyethylene
CHARACTERISTICS:GOOD IMPACT STRENGTH, MEDUIM STIFFNESSGOOD PROCESSABILITYAPPLICATIONS:BLOW MOLDINGFOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES,COSMETIC BOTTLES, CHEMICAL CONTAI..
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene G2865 High Density Polyethylene
CHARACTERISTICS: HIGH STIFFNESS, GOOD IMPACT STRENGTH, GOOD PROCESSABILITYAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DIARY PRODUCT BOTTLES, FRUIT JUICE BOTTLES, ONE-..
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GM2860 High Density Polyethylene
CHARACTERISTICS: HIGH IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH STIFFNESSAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES COSMETIC BOTTLES, ONE-WAY BOTT..
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GM2865 High Density Polyethylene
CHARACTERISTICS: EXCELLENT STIFFNESS, GOOD PROCESSABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DAIRY PRODUCT BOTTLES MILK BOTTLES AND GALL..
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Total HDPE HL 535 High Density Polyethylene, Film Resin
Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release ..
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil HDPE HYA 600 High Density Polyethylene Resin
Product Description: HYA 600 is a general purpose HDPE resin, characterized by very easy processability, an excellent balance of rigidity and impact strength and a good ESCR.Availability: Africa & M..
Melt Flow 0.35 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.35 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ASA S519
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem BS002HS HDPE Blow Molding Polyethylene Copolymer
Resin BS002HS is a high-density polyethylene, bimodal copolymer. It presents good rigidity, good impact resistance, and good reproducibility of the weight of the bottles. It also has excellent envir..