Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.38 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.38 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
SABIC BM1052 High Density Polyethylene for Blow Molding Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high im.. |
|||
Melt Flow | 0.38 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.38 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GF5250 HDPE Blow Molding Polyethylene Copolymer GF5250 is a high-density polyethylene copolymer with well balanced properties between impact and stiffness combined with high productivity and good processability. It was developed for the blow-mold.. |
|||
Melt Flow | 0.38 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.38 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem BU004 Blow Molding High Density Polyethylene Containers for lubricating oils, alcohol, cosmetics and yots; Toys.Information provided by Braskem. |