Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.18 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.18 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Flow | 0.18 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.18 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem ES 002G HDPE Pipe Extrusion Polyethylene
(discontinued **) Applications: Flat and corrugated pipes extrusion for mining, energy and telecommunication systems; piping in sewage systems. Information provided by Braskem |
|||
Melt Flow | 0.18 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.18 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene EX 6HT is a high density polyethylene with 1-Butene as co monomer. It has good toughness, low gel level, good tear strength, high tenacity.Applications: film extrusion, blending partner, refuse ba.. |