Braskem ES 002G HDPE Pipe Extrusion Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem ES 002G HDPE Pipe Extrusion Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Flat and corrugated pipes extrusion for mining, energy and telecommunication systems; piping in sewage systems. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 0.18 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.18 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
0.65 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.65 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength at Break 34.0 MPa
4930 psi
ASTM D638
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Flexural Modulus 1.254 GPa
181.9 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
153 °F
ASTM D648
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Descriptive Properties Value Comments
Molecular Weight Distribution Bimodal