Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.12 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.12 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) BL6 HM7255 High Density Polyethylene BL6 (HM 755) is a high density polyethylene with Butene-1 as a comonomer. It is a high molar mass material with very good impact strength, stiffness, and stress cracking resistance.Applications: la.. |
|||
Melt Flow | 0.12 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene BM3245 PC High Density Polyethylene CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS:PIPE EXTRUSIONSUI.. |