Iran Petrochemical (PCC) BL6 HM7255 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) BL6 HM7255 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BL6 (HM 755) is a high density polyethylene with Butene-1 as a comonomer. It is a high molar mass material with very good impact strength, stiffness, and stress cracking resistance.Applications: larger containers above 5 L, manufacture of semi-finished products.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ISO 1183
Melt Flow 0.12 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.12 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
2.7 g/10 min

@Load 21.6 kg,
Temperature 190 °C
2.7 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Charpy Impact, Notched 4.20 J/cm²
20.0 ft-lb/in²
ISO 179
Descriptive Properties Value Comments
Swell Ratio, % 145
±20