Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA73MP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA73MP is a lubricated and nucleated low viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 C.. |
|||
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA73ZP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combinati.. |
|||
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA95MP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95MP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combinati.. |
|||
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA95QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95QP is a lubricated medium viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500.. |
|||
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA95YP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95YP is a lubricated medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.. |
|||
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA95ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95ZP is a medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It p.. |
|||
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA115QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115QP is a lubricated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500... |
|||
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA115ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115ZP is a high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It possess.. |
|||
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA155MP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115MP is a lubricated and nucleated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21.. |
|||
Oxygen Transmission Rate | 37.2 cc/m²/day | 2.40 cc/100 in²/day | |
Honeywell Aegis™ HCA155QP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115QP is a lubricated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500... |