Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 4900 cc/m²/day | 316 cc/100 in²/day | ASTM D3985 |
Chevron Phillips MarFlex® 5335 Low Density Polyethylene, Blown Film This LDPE is tailored for blown film applications that require:Good processabilityLow coefficient of frictionGood openabilityGood sealabilityTypical blown film applications include:Institutional pac.. |