Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 22.0 - 26.0 cc/m²/day | 1.42 - 1.67 cc/100 in²/day | 73°F (23°C) / 65%RH; ASTM D3985 |
Honeywell Capran® Oxyshield™ M-OPA (1.0 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and.. |