Polymer Property : Oxygen Transmission Rate = 1.42 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 22.0 - 26.0 cc/m²/day
1.42 - 1.67 cc/100 in²/day
73°F (23°C) / 65%RH; ASTM D3985
Honeywell Capran® Oxyshield™ M-OPA (1.0 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film
Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and..