Polymer Property : Oxygen Transmission Rate = 124 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 1920 cc/m²/day
124 cc/100 in²/day
0% RH; ASTM D 1434
NOVA Chemicals Sclair® 17A Butene HDPE Film Resin
17A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te..