Polymer Property : Oxygen Transmission Rate = 1.29 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 2.00 - 20.0 cc/m²/day
0.129 - 1.29 cc/100 in²/day
Average value: 14.0 cc/m²/day Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..