Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 18.6 cc/m²/day

@Temperature 23.0 °C
1.20 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Metallyte™ 12MM281 OPP Film
Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. 12MM281 is designed for use as the center web of a triplex adhesive lamination. The treated s..