Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 1.00 - 2.00 cc/m²/day | 0.0644 - 0.129 cc/100 in²/day | |
UBE 7024B Five Layer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |