Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE 7024B Five Layer Film

Category Polymer , Film , Thermoplastic , Nylon
Manufacturer UBE
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE 7024B Five Layer Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal packagesFlavor barrier (compare with HDPE)Form-fill-seal (Air blown)Information provided by UBE.
Physical Properties Metric English Comments
Oxygen Transmission Rate 1.00 - 2.00 cc/m²/day
0.0644 - 0.129 cc/100 in²/day
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
Film Tensile Strength at Yield, TD 18.0 MPa
2610 psi
Film Elongation at Break, MD 440 %
440 %
Film Elongation at Break, TD 480 %
480 %
Film Tensile Strength at Break, MD 41.0 MPa
5950 psi
Film Tensile Strength at Break, TD 43.0 MPa
6240 psi
Processing Properties Metric English Comments
Processing Temperature 210 °C
410 °F
C1
220 °C
428 °F
C2
220 °C
428 °F
C3
220 °C
428 °F
AD
220 °C
428 °F
F
Descriptive Properties Value Comments
Layer Structure 7024B / Ad / EVOH / Ad/ Surly: (20 / 10 / 20 / 10 / 70 um)
Copyright © lookpolymers.com All Rights Reserved