Physical Properties Metric English Comments
Oxygen Transmission Rate 1.10 cc/m²/day
0.0708 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Honeywell Capran® Emblem™ MT1500 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ MT1500 is a 0.60 mil (15 micron) biaxially oriented nylon 6 film with a metallized barrier coating well suited for high barrier packaging applications. Informati..
Oxygen Transmission Rate 1.10 cc/m²/day
0.0708 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Honeywell Capran® Emblem™ MT2500 Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ MT2500 is a 1.00 mil (25 micron) biaxially oriented nylon 6 film with a metallized barrier coating.Applications: Capron® Emblem™ MT2500 is well suited fo..