Physical Properties Metric English Comments
Water Vapor Transmission 7.92 g/m²/day

@Temperature 38.0 °C
0.510 g/100 in²/day

@Temperature 100 °F
100% RH; ExxonMobil Method
ExxonMobil Bicor™ 18 MAT OPP Film
Product Description: Bicor MAT is a one-side matte finish, one-side treated, non-heat sealable OPP film designed for use as the outer web of a lamination. MAT is also an excellent matte finish slip ..
Water Vapor Transmission 7.92 g/m²/day

@Temperature 38.0 °C
0.510 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 70 CSR-M OPP Film
Product Description: Bicor CSR-M is a one-side matte finish, on-side treated, non-heat sealable OPP film designed for cold seal release as the outer web of a lamination. CSR-M is also an excellent m..