ExxonMobil Bicor™ 70 CSR-M OPP Film

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Bicor™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Bicor™ 70 CSR-M OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Bicor CSR-M is a one-side matte finish, on-side treated, non-heat sealable OPP film designed for cold seal release as the outer web of a lamination. CSR-M is also an excellent matte finish slip film for heat seal laminations. The paper-like appearance of CSR-M provides a differentiated shelf appeal, with a satiny appearance when reverse printed.Availability: Latin America, North America and South AmericaKey Features:Excellent ink adhesion on the treated surfaceNon-migratory slip system for consistent COFVery uniform low-glass surfaceExcellent release from cold seal surfacesApplications:BakeryBiscuits/Cookie/CrackersConfectionery, Chocolate Dairy ProductsFresh ProduceUses:HFFS Flexible Packaging VFFS Flexible PackagingProcessing Method: Cold Seal Adhesive, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Water Vapor Transmission 7.92 g/m²/day

@Temperature 38.0 °C
0.510 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
Thickness 17.8 microns
0.700 mil
ExxonMobil Method
Coating Weight 15.7 g/m²
9.80 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.35
0.35
24 hr, Matte/Matte; ExxonMobil Method
Film Tensile Strength at Break, MD 110 MPa
16000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 207 MPa
30000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.0 %

@Temperature 135 °C
4.0 %

@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 3.0 %

@Temperature 135 °C
3.0 %

@Temperature 275 °F
ExxonMobil Method
Optical Properties Metric English Comments
Haze 72 %
72 %
ExxonMobil Method
Gloss 8.0 %
8.0 %
45°, Matte Surface; ExxonMobil Method
Descriptive Properties Value Comments
Wetting Tension 0.82 receding cos theta
Treated Surface
Yield 44000 in2/lb