Physical Properties Metric English Comments
Water Vapor Transmission 7.60 g/m²/day
0.489 g/100 in²/day
ASTM F1249
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film
Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood ..
Water Vapor Transmission 7.60 g/m²/day
0.489 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
ExxonMobil Bicor® 420 HS OPP Film
Product Description: Bicor HS is a two-side coated, sealable OPP film designed for general use in overwrap and horizontal packaging. This film is suitable as an unsupported web or lamination. It can..