Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 7.60 g/m²/day | 0.489 g/100 in²/day | ASTM F1249 |
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood .. |
|||
Water Vapor Transmission | 7.60 g/m²/day | 0.489 g/100 in²/day | 38°C, 90% RH; ExxonMobil Method |
ExxonMobil Bicor® 420 HS OPP Film Product Description: Bicor HS is a two-side coated, sealable OPP film designed for general use in overwrap and horizontal packaging. This film is suitable as an unsupported web or lamination. It can.. |